Contact Us

SRD-100 microcomputer controlled electronic creep tester

SRD-100 microcomputer-controlled electronic creep tester can perform tensile, creep, long-lasting and stress relaxation tests on metal non-metal materials under certain temperature conditions, and can also perform low cycle fatigue and creep fatigue tests. Mainly used in the measurement of quality inspection, aerospace, metallurgical steel, colleges and universities and research laboratories and other industrial sectors.

SRD-100 microcomputer-controlled electronic creep tester can perform tensile, creep, long-lasting and stress relaxation tests on metal non-metal materials under certain temperature conditions, and can also perform low cycle fatigue and creep fatigue tests. Mainly used in the measurement of quality inspection, aerospace, metallurgical steel, colleges and universities and research laboratories and other industrial sectors.

 

Spesification

 

Serial number

project name

Technical Parameters

1

Maximum test force (kN)

100

2

level of accuracy

0.5 level / 1 level

3

Test force measurement range

1% to 100% FS

4

Test force relative value

±0.5%/±1%

5

Test force resolution

1/240000 (no change in the whole range)

6

Concentricity

≤10%

7

Deformation measurement error

±0.002mm (grating sensor)

8

Pull rod maximum stroke

150mm

9

Tie rod speed

0.01~50mm/min

10

Mainframe dimensions (length × width × height) mm

820×500×2360

11

Host weight (kg)

520

12

Temperature range (°C)

200~1100

13

Temperature fluctuation (°C)

±2

14

Average tropical length (mm)

150

15

Temperature gradient (°C)

3

Punya pertanyaan? Tanya asisten AI kami atau chat tim kami.WhatsApp